Automatic shot-blasting makes it possible to obtain a surface condition of the offcuts without oxidation and scale.
These process of systematic pickling of scraps after drawing is essential for the vacuum foundry.
At the end of the chain, each batch is systematically checked by sampling and analyzed quantitatively in order to establish and provide a specific certificate of analysis.